Backtested Material Engineering Datasheet

1,4-Dioxane vs Buna-N Compatibility

Verified chemical resistance rating (Incompatible — Immediate Failure Risk), thermal boundary limits (Not recommended at any temperature or concentration), and material specification guide for Buna-N exposed to 1,4-Dioxane in Polar Organic Solvent (Ketone / Ester / Ether) service.

Official Resistance Rating Grade D
D-Severe Effect Incompatible — Immediate Failure Risk
Buna-N D-Severe Effect
Engineering Verdict — Incompatible — Immediate Failure Risk D-Severe Effect

1,4-Dioxane vs Buna-N: D-Severe Effect

Exposing Buna-N to 1,4-Dioxane (Formula: C4H8O2, CAS: 123-91-1) carries an official rating of D-Severe Effect (Incompatible — Immediate Failure Risk). Maximum recommended thermal operating limit: Not recommended at any temperature or concentration. Best Grade A alternative materials for continuous or high-temperature service: Stainless Steel, PTFE.

Verification Audit: Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Technical Specifications and Operating Parameters

Chemical Medium 1,4-Dioxane
Chemical Formula C4H8O2
CAS Registry Number 123-91-1
Chemical Functional Class Polar Organic Solvent (Ketone / Ester / Ether)
Wetted Material Buna-N
Official Resistance Rating D-Severe Effect (Grade D)
Engineering Service Verdict Incompatible — Immediate Failure Risk
Max Temp and Concentration Limit Not recommended at any temperature or concentration
Best Grade A Alternatives Stainless Steel, PTFE
Backtest and Audit Verification Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

1,4-Dioxane Cross-Material Comparison Matrix (9 Materials)

Direct benchmark ratings across all 9 reference industrial materials for 1,4-Dioxane:

Polypropylene B1-Good
316 Stainless Steel A-Excellent
Viton (FKM) D-Severe Effect
PTFE (Teflon) A-Excellent
EPDM B1-Good
PVC Type I D-Severe Effect
PVDF (Kynar) C-Fair
Buna-N (Nitrile) D-Severe Effect
HDPE B1-Good
Material Name Compatibility Rating Service Verdict Temperature Limit Datasheet
Buna-N D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
EPDM B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
HDPE B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
Polypropylene B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
PTFE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVC D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
PVDF C-Fair Caution: Limited / Intermittent Service Only Ambient intermittent contact only; do not pressurize Report
Stainless Steel A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Viton D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
Buna-N D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
EPDM B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
HDPE B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
Polypropylene B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
PTFE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVC D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
PVDF C-Fair Caution: Limited / Intermittent Service Only Ambient intermittent contact only; do not pressurize Report
Stainless Steel A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Viton D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report

Chemical and Material Interaction Analysis

Engineering Compatibility Verdict

1,4-Dioxane vs Buna-N: D – Severe Effect (Do Not Use)

Summary Verdict: Buna-N (Nitrile / NBR Elastomer) is rated D-Severe Effect (Incompatible — Immediate Failure Risk) when exposed to 1,4-Dioxane (Formula: C4H8O2, CAS: 123-91-1). PROHIBITED for wetted service. Immediately substitute with an A-rated material shown in the cross-material comparison table below.

Quick Engineering Specifications

Chemical Media1,4-Dioxane
Chemical FormulaC4H8O2
CAS Registry Number123-91-1
Chemical ClassificationPolar Organic Solvent (Ketone / Ester / Ether)
Wetted MaterialBuna-N (Nitrile / NBR Elastomer) (Acrylonitrile-Butadiene Copolymer Elastomer)
Official Resistance RatingD – Severe Effect (Do Not Use) (Grade D)
Recommended Temperature WindowNot recommended at any temperature or concentration (Material limit: -40°F to 250°F (-40°C to 121°C))
Top Grade-A AlternativesStainless Steel, PTFE
Data Verification StatusVerified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Chemical & Material Interaction Analysis

1,4-Dioxane is classified as a polar organic solvent (ketone / ester / ether) (strong solvation power that rapidly swells or dissolves many elastomers and amorphous thermoplastics). Used in industrial degreasing, coatings, resin dissolution, and pharmaceutical extraction. When selecting wetted components for Buna-N, engineers must account for both concentration-dependent chemical attack and thermal stress:

  • Reaction & Failure Mechanism: Causes rapid, catastrophic material failure—including severe dissolution, stress cracking, extreme volumetric blowout (>25% swell), or rapid pitting corrosion (>50 mpy).
  • Material Profile (Buna-N): Workhorse elastomer for petroleum-based hydraulic oils, motor oils, diesel, gasoline, aliphatic hydrocarbons (hexane, heptane), water, and salt brines. However, poor resistance to ozone/weathering and rapidly destroyed by ketones, esters, chlorinated hydrocarbons, aromatic solvents, and strong oxidizing acids.
  • Application Scope: Common wetted components include hydraulic O-rings, fuel transfer hoses, rotary shaft seals, oil gaskets, and general-purpose industrial pump elastomers.

Cross-Material Compatibility Comparison for 1,4-Dioxane

To help you select the longest-lasting piping, valve lining, or O-ring seal for 1,4-Dioxane, the table below compares Buna-N against 8 other common industrial engineering materials:

Wetted Material Compatibility Rating Service Recommendation Material Temp Range
Polypropylene (PP Homopolymer & Copolymer)B1-GoodAcceptable with Routine Inspection32°F to 180°F (0°C to 82°C)
316 / 304 Austenitic Stainless SteelA-ExcellentSafe for Continuous Industrial Service-325°F to 800°F (-198°C to 426°C)
Viton® (FKM Fluoroelastomer)D-Severe EffectIncompatible — Immediate Failure Risk-15°F to 400°F (-26°C to 204°C)
PTFE (Teflon® / Polytetrafluoroethylene)A-ExcellentSafe for Continuous Industrial Service-328°F to 500°F (-200°C to 260°C)
EPDM (Ethylene Propylene Diene Monomer)B1-GoodAcceptable with Routine Inspection-60°F to 300°F (-51°C to 149°C)
PVC Type I (Unplasticized Polyvinyl Chloride / uPVC)D-Severe EffectIncompatible — Immediate Failure Risk32°F to 140°F (0°C to 60°C)
PVDF (Kynar® / Polyvinylidene Fluoride)C-FairCaution: Limited / Intermittent Service Only-40°F to 280°F (-40°C to 138°C)
Buna-N (Nitrile / NBR Elastomer) (Current Page)D-Severe EffectIncompatible — Immediate Failure Risk-40°F to 250°F (-40°C to 121°C)
HDPE (High-Density Polyethylene)B1-GoodAcceptable with Routine Inspection-60°F to 140°F (-51°C to 60°C)

Frequently Asked Questions (FAQ)

Is Buna-N compatible with 1,4-Dioxane?

Buna-N is rated D-Severe Effect (Incompatible — Immediate Failure Risk) with 1,4-Dioxane (Formula: C4H8O2, CAS: 123-91-1). Causes rapid, catastrophic material failure—including severe dissolution, stress cracking, extreme volumetric blowout (>25% swell), or rapid pitting corrosion (>50 mpy). PROHIBITED for wetted service. Immediately substitute with an A-rated material shown in the cross-material comparison table below.

What is the best alternative material for handling 1,4-Dioxane?

If Buna-N does not meet your temperature or pressure requirements for 1,4-Dioxane, the highest-rated Grade A alternatives are Stainless Steel, PTFE. Always verify O-ring elastomers and metallic fasteners separately before full-scale deployment.

Technical Engineering FAQs: 1,4-Dioxane vs Buna-N

Click any question below for chemical failure-mode specifics, thermal derating limits, and material selection rules:

Can Buna-N be specified for 1,4-Dioxane process piping, valves, or gaskets?
Do not specify Buna-N for wetted service with 1,4-Dioxane. It carries a Grade D (D-Severe Effect) rating (Incompatible — Immediate Failure Risk) due to rapid chemical attack, severe swelling, stress cracking, or structural dissolution. Substitute with Grade A materials such as Stainless Steel, PTFE.
How do all 9 reference materials compare for 1,4-Dioxane (CAS 123-91-1)?
For 1,4-Dioxane (C4H8O2, Polar Organic Solvent (Ketone / Ester / Ether)), our cross-material compatibility matrix establishes the following ratings across all 9 engineering materials: Polypropylene: B1-Good | 316 Stainless Steel: A-Excellent | PTFE (Teflon): A-Excellent | PVDF (Kynar): C-Fair | PVC Type I: D-Severe Effect | HDPE: B1-Good | Viton (FKM): D-Severe Effect | EPDM: B1-Good | Buna-N (Nitrile): D-Severe Effect.