Backtested Material Engineering Datasheet

Acetic Acid 80% vs Buna-N Compatibility

CAS: 64-19-7 Formula: CH3COOH (80% aq.) Chemical: Acetic Acid 80% Material: Buna-N Grade C

Verified chemical resistance rating (Caution: Limited / Intermittent Service Only), thermal boundary limits (Ambient intermittent contact only; do not pressurize), and material specification guide for Buna-N exposed to Acetic Acid 80% in Organic / Weak Mineral Acid service.

Official Resistance Rating Grade C
C-Fair Caution: Limited / Intermittent Service Only
Buna-N C-Fair
Engineering Verdict — Caution: Limited / Intermittent Service Only C-Fair

Acetic Acid 80% vs Buna-N: C-Fair

Exposing Buna-N to Acetic Acid 80% (Formula: CH3COOH (80% aq.), CAS: 64-19-7) carries an official rating of C-Fair (Caution: Limited / Intermittent Service Only). Maximum recommended thermal operating limit: Ambient intermittent contact only; do not pressurize. Best Grade A alternative materials for continuous or high-temperature service: Polypropylene, PTFE, EPDM, PVC.

Verification Audit: Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Technical Specifications and Operating Parameters

Chemical Medium Acetic Acid 80%
Chemical Formula CH3COOH (80% aq.)
CAS Registry Number 64-19-7
Chemical Functional Class Organic / Weak Mineral Acid
Wetted Material Buna-N
Official Resistance Rating C-Fair (Grade C)
Engineering Service Verdict Caution: Limited / Intermittent Service Only
Max Temp and Concentration Limit Ambient intermittent contact only; do not pressurize
Best Grade A Alternatives Polypropylene, PTFE, EPDM, PVC
Backtest and Audit Verification Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Acetic Acid 80% Cross-Material Comparison Matrix (9 Materials)

Direct benchmark ratings across all 9 reference industrial materials for Acetic Acid 80%:

Polypropylene A-Excellent
316 Stainless Steel D-Severe Effect
Viton (FKM) B-Good
PTFE (Teflon) A-Excellent
EPDM A-Excellent
PVC Type I A-Excellent
PVDF (Kynar) A-Excellent
Buna-N (Nitrile) C-Fair
HDPE A-Excellent
Material Name Compatibility Rating Service Verdict Temperature Limit Datasheet
Buna-N C-Fair Caution: Limited / Intermittent Service Only Ambient intermittent contact only; do not pressurize Report
EPDM A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
HDPE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Polypropylene A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PTFE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVC A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVDF A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Stainless Steel D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
Viton B-Good Acceptable with Operating Controls Ambient service (72°F / 22°C) preferred; monitor wear in continuous service Report

Chemical and Material Interaction Analysis

Engineering Compatibility Verdict

Acetic Acid 80% vs Buna-N: C – Fair (Moderate Effect / Not Recommended for Continuous Duty)

Summary Verdict: Buna-N (Nitrile / NBR Elastomer) is rated C-Fair (Caution: Limited / Intermittent Service Only) when exposed to Acetic Acid 80% (Formula: CH3COOH (80% aq.), CAS: 64-19-7). Do not specify for primary containment or pressurized lines. Select an A-rated alternative from the comparison matrix below.

Quick Engineering Specifications

Chemical MediaAcetic Acid 80%
Chemical FormulaCH3COOH (80% aq.)
CAS Registry Number64-19-7
Chemical ClassificationOrganic / Weak Mineral Acid
Wetted MaterialBuna-N (Nitrile / NBR Elastomer) (Acrylonitrile-Butadiene Copolymer Elastomer)
Official Resistance RatingC – Fair (Moderate Effect / Not Recommended for Continuous Duty) (Grade C)
Recommended Temperature WindowAmbient intermittent contact only; do not pressurize (Material limit: -40°F to 250°F (-40°C to 121°C))
Top Grade-A AlternativesPolypropylene, PTFE, EPDM, PVC
Data Verification StatusVerified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Chemical & Material Interaction Analysis

Acetic Acid 80% is classified as an organic / weak mineral acid (mild to moderate acidic hydrolysis and potential elastomer swelling). Used in food processing, pharmaceutical formulation, buffering, and industrial cleaning. When selecting wetted components for Buna-N, engineers must account for both concentration-dependent chemical attack and thermal stress:

  • Reaction & Failure Mechanism: Triggers progressive mechanical degradation, plasticizer extraction, elastomeric swell, or localized corrosion over multi-day exposure.
  • Material Profile (Buna-N): Workhorse elastomer for petroleum-based hydraulic oils, motor oils, diesel, gasoline, aliphatic hydrocarbons (hexane, heptane), water, and salt brines. However, poor resistance to ozone/weathering and rapidly destroyed by ketones, esters, chlorinated hydrocarbons, aromatic solvents, and strong oxidizing acids.
  • Application Scope: Common wetted components include hydraulic O-rings, fuel transfer hoses, rotary shaft seals, oil gaskets, and general-purpose industrial pump elastomers.

Cross-Material Compatibility Comparison for Acetic Acid 80%

To help you select the longest-lasting piping, valve lining, or O-ring seal for Acetic Acid 80%, the table below compares Buna-N against 8 other common industrial engineering materials:

Wetted Material Compatibility Rating Service Recommendation Material Temp Range
Polypropylene (PP Homopolymer & Copolymer)A-ExcellentSafe for Continuous Industrial Service32°F to 180°F (0°C to 82°C)
316 / 304 Austenitic Stainless SteelD-Severe EffectIncompatible — Immediate Failure Risk-325°F to 800°F (-198°C to 426°C)
Viton® (FKM Fluoroelastomer)B-GoodAcceptable with Operating Controls-15°F to 400°F (-26°C to 204°C)
PTFE (Teflon® / Polytetrafluoroethylene)A-ExcellentSafe for Continuous Industrial Service-328°F to 500°F (-200°C to 260°C)
EPDM (Ethylene Propylene Diene Monomer)A-ExcellentSafe for Continuous Industrial Service-60°F to 300°F (-51°C to 149°C)
PVC Type I (Unplasticized Polyvinyl Chloride / uPVC)A-ExcellentSafe for Continuous Industrial Service32°F to 140°F (0°C to 60°C)
PVDF (Kynar® / Polyvinylidene Fluoride)A-ExcellentSafe for Continuous Industrial Service-40°F to 280°F (-40°C to 138°C)
Buna-N (Nitrile / NBR Elastomer) (Current Page)C-FairCaution: Limited / Intermittent Service Only-40°F to 250°F (-40°C to 121°C)
HDPE (High-Density Polyethylene)A-ExcellentSafe for Continuous Industrial Service-60°F to 140°F (-51°C to 60°C)

Frequently Asked Questions (FAQ)

Is Buna-N compatible with Acetic Acid 80%?

Buna-N is rated C-Fair (Caution: Limited / Intermittent Service Only) with Acetic Acid 80% (Formula: CH3COOH (80% aq.), CAS: 64-19-7). Triggers progressive mechanical degradation, plasticizer extraction, elastomeric swell, or localized corrosion over multi-day exposure. Do not specify for primary containment or pressurized lines. Select an A-rated alternative from the comparison matrix below.

What is the best alternative material for handling Acetic Acid 80%?

If Buna-N does not meet your temperature or pressure requirements for Acetic Acid 80%, the highest-rated Grade A alternatives are Polypropylene, PTFE, EPDM, PVC. Always verify O-ring elastomers and metallic fasteners separately before full-scale deployment.

Technical Engineering FAQs: Acetic Acid 80% vs Buna-N

Click any question below for chemical failure-mode specifics, thermal derating limits, and material selection rules:

Can Buna-N be specified for Acetic Acid 80% process piping, valves, or gaskets?
Exercise caution. Buna-N carries a Grade C (C-Fair) rating in Acetic Acid 80% service (Caution: Limited / Intermittent Service Only). Moderate swelling, mechanical softening, or measurable corrosion occurs under continuous exposure. Restrict use to short-term ambient contact (Ambient intermittent contact only; do not pressurize), and specify Polypropylene, PTFE, EPDM, PVC for permanent installations.
How do all 9 reference materials compare for Acetic Acid 80% (CAS 64-19-7)?
For Acetic Acid 80% (CH3COOH (80% aq.), Organic / Weak Mineral Acid), our cross-material compatibility matrix establishes the following ratings across all 9 engineering materials: Polypropylene: A-Excellent | 316 Stainless Steel: D-Severe Effect | PTFE (Teflon): A-Excellent | PVDF (Kynar): A-Excellent | PVC Type I: A-Excellent | HDPE: A-Excellent | Viton (FKM): B-Good | EPDM: A-Excellent | Buna-N (Nitrile): C-Fair.