Backtested Material Engineering Datasheet

Cyclohexylamine vs HDPE Compatibility

CAS: 108-91-8 Formula: C6H11NH2 (C6H13N) Chemical: Cyclohexylamine Material: HDPE Grade B

Verified chemical resistance rating (Acceptable with Routine Inspection), thermal boundary limits (Up to 120°F (49°C) with minor absorption/corrosion allowance), and material specification guide for HDPE exposed to Cyclohexylamine in Alkaline Base / Amine service.

Official Resistance Rating Grade B
B1-Good Acceptable with Routine Inspection
HDPE B1-Good
Engineering Verdict — Acceptable with Routine Inspection B1-Good

Cyclohexylamine vs HDPE: B1-Good

Exposing HDPE to Cyclohexylamine (Formula: C6H11NH2 (C6H13N), CAS: 108-91-8) carries an official rating of B1-Good (Acceptable with Routine Inspection). Maximum recommended thermal operating limit: Up to 120°F (49°C) with minor absorption/corrosion allowance. Best Grade A alternative materials for continuous or high-temperature service: Stainless Steel, PTFE.

Verification Audit: Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Technical Specifications and Operating Parameters

Chemical Medium Cyclohexylamine
Chemical Formula C6H11NH2 (C6H13N)
CAS Registry Number 108-91-8
Chemical Functional Class Alkaline Base / Amine
Wetted Material HDPE
Official Resistance Rating B1-Good (Grade B)
Engineering Service Verdict Acceptable with Routine Inspection
Max Temp and Concentration Limit Up to 120°F (49°C) with minor absorption/corrosion allowance
Best Grade A Alternatives Stainless Steel, PTFE
Backtest and Audit Verification Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Cyclohexylamine Cross-Material Comparison Matrix (9 Materials)

Direct benchmark ratings across all 9 reference industrial materials for Cyclohexylamine:

Polypropylene B1-Good
316 Stainless Steel A-Excellent
Viton (FKM) D-Severe Effect
PTFE (Teflon) A-Excellent
EPDM B1-Good
PVC Type I D-Severe Effect
PVDF (Kynar) C-Fair
Buna-N (Nitrile) C-Fair
HDPE B1-Good
Material Name Compatibility Rating Service Verdict Temperature Limit Datasheet
Buna-N C-Fair Caution: Limited / Intermittent Service Only Ambient intermittent contact only; do not pressurize Report
EPDM B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
HDPE B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
Polypropylene B1-Good Acceptable with Routine Inspection Up to 120°F (49°C) with minor absorption/corrosion allowance Report
PTFE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVC D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report
PVDF C-Fair Caution: Limited / Intermittent Service Only Ambient intermittent contact only; do not pressurize Report
Stainless Steel A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Viton D-Severe Effect Incompatible — Immediate Failure Risk Not recommended at any temperature or concentration Report

Chemical and Material Interaction Analysis

Engineering Compatibility Verdict

Cyclohexylamine vs HDPE: B1 – Good (Minor Effect up to 120°F / 49°C)

Summary Verdict: HDPE (High-Density Polyethylene) is rated B1-Good (Acceptable with Routine Inspection) when exposed to Cyclohexylamine (Formula: C6H11NH2 (C6H13N), CAS: 108-91-8). Suitable for secondary transfer lines, static gaskets, and intermittent batch service. Avoid thin-walled high-stress dynamic seals without prior coupon testing.

Quick Engineering Specifications

Chemical MediaCyclohexylamine
Chemical FormulaC6H11NH2 (C6H13N)
CAS Registry Number108-91-8
Chemical ClassificationAlkaline Base / Amine
Wetted MaterialHDPE (High-Density Polyethylene) (Linear Semi-Crystalline Polyolefin Thermoplastic)
Official Resistance RatingB1 – Good (Minor Effect up to 120°F / 49°C) (Grade B)
Recommended Temperature WindowUp to 120°F (49°C) with minor absorption/corrosion allowance (Material limit: -60°F to 140°F (-51°C to 60°C))
Top Grade-A AlternativesStainless Steel, PTFE
Data Verification StatusVerified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Chemical & Material Interaction Analysis

Cyclohexylamine is classified as an alkaline base / amine (high-pH alkaline attack, stress-corrosion risk at high temperatures, and dehydrofluorination of fluoroelastomers). Used in caustic scrubbing, CIP (Clean-in-Place) sanitation, neutralization, and chemical synthesis. When selecting wetted components for HDPE, engineers must account for both concentration-dependent chemical attack and thermal stress:

  • Reaction & Failure Mechanism: Causes slight surface absorption, minor weight gain (1%–5% swell in polymers), or a low corrosion rate (<2 to 20 mpy in metals) up to 120°F (49°C).
  • Material Profile (HDPE): High impact strength (even at sub-zero temperatures) and excellent resistance to mineral acids, caustics, salt brines, and alcohols. However, lower upper temperature limit (140°F/60°C) than Polypropylene, with susceptibility to permeation and environmental stress cracking in aromatic/chlorinated hydrocarbons and strong oxidizers.
  • Application Scope: Common wetted components include bulk chemical storage tanks, IBC totes, double-containment underground piping, and chemical drum liners.

Cross-Material Compatibility Comparison for Cyclohexylamine

To help you select the longest-lasting piping, valve lining, or O-ring seal for Cyclohexylamine, the table below compares HDPE against 8 other common industrial engineering materials:

Wetted Material Compatibility Rating Service Recommendation Material Temp Range
Polypropylene (PP Homopolymer & Copolymer)B1-GoodAcceptable with Routine Inspection32°F to 180°F (0°C to 82°C)
316 / 304 Austenitic Stainless SteelA-ExcellentSafe for Continuous Industrial Service-325°F to 800°F (-198°C to 426°C)
Viton® (FKM Fluoroelastomer)D-Severe EffectIncompatible — Immediate Failure Risk-15°F to 400°F (-26°C to 204°C)
PTFE (Teflon® / Polytetrafluoroethylene)A-ExcellentSafe for Continuous Industrial Service-328°F to 500°F (-200°C to 260°C)
EPDM (Ethylene Propylene Diene Monomer)B1-GoodAcceptable with Routine Inspection-60°F to 300°F (-51°C to 149°C)
PVC Type I (Unplasticized Polyvinyl Chloride / uPVC)D-Severe EffectIncompatible — Immediate Failure Risk32°F to 140°F (0°C to 60°C)
PVDF (Kynar® / Polyvinylidene Fluoride)C-FairCaution: Limited / Intermittent Service Only-40°F to 280°F (-40°C to 138°C)
Buna-N (Nitrile / NBR Elastomer)C-FairCaution: Limited / Intermittent Service Only-40°F to 250°F (-40°C to 121°C)
HDPE (High-Density Polyethylene) (Current Page)B1-GoodAcceptable with Routine Inspection-60°F to 140°F (-51°C to 60°C)

Frequently Asked Questions (FAQ)

Is HDPE compatible with Cyclohexylamine?

HDPE is rated B1-Good (Acceptable with Routine Inspection) with Cyclohexylamine (Formula: C6H11NH2 (C6H13N), CAS: 108-91-8). Causes slight surface absorption, minor weight gain (1%–5% swell in polymers), or a low corrosion rate (<2 to 20 mpy in metals) up to 120°F (49°C). Suitable for secondary transfer lines, static gaskets, and intermittent batch service. Avoid thin-walled high-stress dynamic seals without prior coupon testing.

What is the best alternative material for handling Cyclohexylamine?

If HDPE does not meet your temperature or pressure requirements for Cyclohexylamine, the highest-rated Grade A alternatives are Stainless Steel, PTFE. Always verify O-ring elastomers and metallic fasteners separately before full-scale deployment.

Technical Engineering FAQs: Cyclohexylamine vs HDPE

Click any question below for chemical failure-mode specifics, thermal derating limits, and material selection rules:

Can HDPE be specified for Cyclohexylamine process piping, valves, or gaskets?
HDPE is rated Grade B (B1-Good) for Cyclohexylamine (Acceptable with Routine Inspection). It is suitable for secondary transfer lines, static gaskets, and intermittent batch service up to Up to 120°F (49°C) with minor absorption/corrosion allowance with routine inspection. For high-stress dynamic seals or higher temperatures, upgrade to Stainless Steel, PTFE.
How do all 9 reference materials compare for Cyclohexylamine (CAS 108-91-8)?
For Cyclohexylamine (C6H11NH2 (C6H13N), Alkaline Base / Amine), our cross-material compatibility matrix establishes the following ratings across all 9 engineering materials: Polypropylene: B1-Good | 316 Stainless Steel: A-Excellent | PTFE (Teflon): A-Excellent | PVDF (Kynar): C-Fair | PVC Type I: D-Severe Effect | HDPE: B1-Good | Viton (FKM): D-Severe Effect | EPDM: B1-Good | Buna-N (Nitrile): C-Fair.