Uric Acid vs EPDM Compatibility

Verified chemical resistance rating (Acceptable with Operating Controls), thermal boundary limits (Ambient service (72°F / 22°C) preferred; monitor wear in continuous service), and material specification guide for EPDM exposed to Uric Acid in Organic / Weak Mineral Acid service.

Official Resistance Rating Grade B
B-Good Acceptable with Operating Controls
EPDM B-Good
Engineering Verdict — Acceptable with Operating Controls B-Good

Uric Acid vs EPDM: B-Good

Exposing EPDM to Uric Acid (Formula: C5H4N4O3, CAS: 69-93-2) carries an official rating of B-Good (Acceptable with Operating Controls). Maximum recommended thermal operating limit: Ambient service (72°F / 22°C) preferred; monitor wear in continuous service. Best Grade A alternative materials for continuous or high-temperature service: Polypropylene, Viton, PTFE, PVC.

Verification Audit: Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Technical Specifications and Operating Parameters

Chemical Medium Uric Acid
Chemical Formula C5H4N4O3
CAS Registry Number 69-93-2
Chemical Functional Class Organic / Weak Mineral Acid
Wetted Material EPDM
Official Resistance Rating B-Good (Grade B)
Engineering Service Verdict Acceptable with Operating Controls
Max Temp and Concentration Limit Ambient service (72°F / 22°C) preferred; monitor wear in continuous service
Best Grade A Alternatives Polypropylene, Viton, PTFE, PVC
Backtest and Audit Verification Verified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Uric Acid Cross-Material Comparison Matrix (9 Materials)

Direct benchmark ratings across all 9 reference industrial materials for Uric Acid:

Polypropylene A-Excellent
316 Stainless Steel B-Good
Viton (FKM) A-Excellent
PTFE (Teflon) A-Excellent
EPDM B-Good
PVC Type I A-Excellent
PVDF (Kynar) A-Excellent
Buna-N (Nitrile) B-Good
HDPE A-Excellent
Material Name Compatibility Rating Service Verdict Temperature Limit Datasheet
Buna-N B-Good Acceptable with Operating Controls Ambient service (72°F / 22°C) preferred; monitor wear in continuous service Report
EPDM B-Good Acceptable with Operating Controls Ambient service (72°F / 22°C) preferred; monitor wear in continuous service Report
HDPE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Polypropylene A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PTFE A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVC A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
PVDF A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report
Stainless Steel B-Good Acceptable with Operating Controls Ambient service (72°F / 22°C) preferred; monitor wear in continuous service Report
Viton A-Excellent Safe for Continuous Industrial Service Ambient to elevated operating temperatures within standard material limits Report

Chemical and Material Interaction Analysis

Engineering Compatibility Verdict

Uric Acid vs EPDM: B – Good (Minor Effect / Conditional)

Summary Verdict: EPDM (Ethylene Propylene Diene Monomer) is rated B-Good (Acceptable with Operating Controls) when exposed to Uric Acid (Formula: C5H4N4O3, CAS: 69-93-2). Acceptable for low-pressure piping, static seals, and scheduled-maintenance components. Implement periodic visual and dimensional inspection.

Quick Engineering Specifications

Chemical MediaUric Acid
Chemical FormulaC5H4N4O3
CAS Registry Number69-93-2
Chemical ClassificationOrganic / Weak Mineral Acid
Wetted MaterialEPDM (Ethylene Propylene Diene Monomer) (Synthetic Polar-Service Elastomer)
Official Resistance RatingB – Good (Minor Effect / Conditional) (Grade B)
Recommended Temperature WindowAmbient service (72°F / 22°C) preferred; monitor wear in continuous service (Material limit: -60°F to 300°F (-51°C to 149°C))
Top Grade-A AlternativesPolypropylene, Viton, PTFE, PVC
Data Verification StatusVerified against Cole-Parmer, ISM, Graco & CP Lab Safety industrial chemical resistance charts.

Chemical & Material Interaction Analysis

Uric Acid is classified as an organic / weak mineral acid (mild to moderate acidic hydrolysis and potential elastomer swelling). Used in food processing, pharmaceutical formulation, buffering, and industrial cleaning. When selecting wetted components for EPDM, engineers must account for both concentration-dependent chemical attack and thermal stress:

  • Reaction & Failure Mechanism: Exhibits minor chemical interaction—such as slight discoloration, mild dimensional swell, or slow uniform surface etching—that does not immediately compromise structural integrity.
  • Material Profile (EPDM): Outstanding resistance to polar fluids including ketones (acetone, MEK), alcohols, glycols, phosphate ester hydraulic fluids (Skydrol), alkalis, and dilute acids. However, exhibits rapid, catastrophic volumetric swelling and softening when exposed to petroleum oils, gasoline, diesel, kerosene, aliphatic/aromatic hydrocarbons, and chlorinated solvents.
  • Application Scope: Common wetted components include butterfly valve liners, O-rings, sanitary Tri-Clamp gaskets, caustic dosing hoses, and water/wastewater treatment seals.

Cross-Material Compatibility Comparison for Uric Acid

To help you select the longest-lasting piping, valve lining, or O-ring seal for Uric Acid, the table below compares EPDM against 8 other common industrial engineering materials:

Wetted Material Compatibility Rating Service Recommendation Material Temp Range
Polypropylene (PP Homopolymer & Copolymer)A-ExcellentSafe for Continuous Industrial Service32°F to 180°F (0°C to 82°C)
316 / 304 Austenitic Stainless SteelB-GoodAcceptable with Operating Controls-325°F to 800°F (-198°C to 426°C)
Viton® (FKM Fluoroelastomer)A-ExcellentSafe for Continuous Industrial Service-15°F to 400°F (-26°C to 204°C)
PTFE (Teflon® / Polytetrafluoroethylene)A-ExcellentSafe for Continuous Industrial Service-328°F to 500°F (-200°C to 260°C)
EPDM (Ethylene Propylene Diene Monomer) (Current Page)B-GoodAcceptable with Operating Controls-60°F to 300°F (-51°C to 149°C)
PVC Type I (Unplasticized Polyvinyl Chloride / uPVC)A-ExcellentSafe for Continuous Industrial Service32°F to 140°F (0°C to 60°C)
PVDF (Kynar® / Polyvinylidene Fluoride)A-ExcellentSafe for Continuous Industrial Service-40°F to 280°F (-40°C to 138°C)
Buna-N (Nitrile / NBR Elastomer)B-GoodAcceptable with Operating Controls-40°F to 250°F (-40°C to 121°C)
HDPE (High-Density Polyethylene)A-ExcellentSafe for Continuous Industrial Service-60°F to 140°F (-51°C to 60°C)

Frequently Asked Questions (FAQ)

Is EPDM compatible with Uric Acid?

EPDM is rated B-Good (Acceptable with Operating Controls) with Uric Acid (Formula: C5H4N4O3, CAS: 69-93-2). Exhibits minor chemical interaction—such as slight discoloration, mild dimensional swell, or slow uniform surface etching—that does not immediately compromise structural integrity. Acceptable for low-pressure piping, static seals, and scheduled-maintenance components. Implement periodic visual and dimensional inspection.

What is the best alternative material for handling Uric Acid?

If EPDM does not meet your temperature or pressure requirements for Uric Acid, the highest-rated Grade A alternatives are Polypropylene, Viton, PTFE, PVC. Always verify O-ring elastomers and metallic fasteners separately before full-scale deployment.

Technical Engineering FAQs: Uric Acid vs EPDM

Click any question below for chemical failure-mode specifics, thermal derating limits, and material selection rules:

Can EPDM be specified for Uric Acid process piping, valves, or gaskets?
EPDM is rated Grade B (B-Good) for Uric Acid (Acceptable with Operating Controls). It is suitable for secondary transfer lines, static gaskets, and intermittent batch service up to Ambient service (72°F / 22°C) preferred; monitor wear in continuous service with routine inspection. For high-stress dynamic seals or higher temperatures, upgrade to Polypropylene, Viton, PTFE, PVC.
How do all 9 reference materials compare for Uric Acid (CAS 69-93-2)?
For Uric Acid (C5H4N4O3, Organic / Weak Mineral Acid), our cross-material compatibility matrix establishes the following ratings across all 9 engineering materials: Polypropylene: A-Excellent | 316 Stainless Steel: B-Good | PTFE (Teflon): A-Excellent | PVDF (Kynar): A-Excellent | PVC Type I: A-Excellent | HDPE: A-Excellent | Viton (FKM): A-Excellent | EPDM: B-Good | Buna-N (Nitrile): B-Good.